02
Composition, GSM, construction & finish:
Four fields do most of the work.
If you only ever get fluent in these, you can evaluate 90% of streetwear fabrics with confidence.
Here’s what each one really controls and the traps inside each.
Composition: what it’s made of
Composition is the fiber content and ratio.
It sets the baseline for feel, durability, stretch, care, and cost. In streetwear, you’ll mostly see a handful:
- 100% cotton: soft, breathable, and takes print and dye beautifully, the streetwear default. Shrinks and creases more; costs vary hugely by yarn quality.
- Cotton/polyester (e.g., 80/20, 50/50): poly adds durability, reduces shrinkage and price, and helps fleece keep its shape. The trade-off is a slightly less premium, less breathable hand.
- Cotton/elastane (e.g., 95/5): a touch of elastane for stretch and recovery, common in fitted tees and ribbing.
- Poly/cotton/elastane tri-blends: soft, drapey, marled looks; popular for elevated basics.
- Recycled / organic variants, recycled polyester (rPET), or organic cotton carry a cost premium and a claim you must be able to document.
The trap: ratios are money.
Shifting from 100% cotton to 65/35 cotton/poly changes cost, shrinkage, and hand all three.
“Cotton-rich” or “cotton blend” on a spec is a red flag; make the supplier state the exact split.
Fabric content: what the label means, and how to check it
Fabric content is the same as composition, seen from the other side.
On a spec sheet, it’s called composition. On the sewn-in label, it’s called fabric content (or fiber content).
It means one thing: which fibers the fabric is made of and what share of the total weight each one is.
So “80% cotton, 20% polyester” means 80% of the fabric’s weight is cotton, and 20% is polyester.
It isn’t a thread count. And it says nothing about weight, yarn, or quality. A 100% cotton tee can still be thin, rough, and cheap.
How a fabric content label is written
The rules are close to identical in the US, EU, UK, and Canada:
- Every fiber at 5% or more is listed, as a percentage of total weight.
- Largest fiber first, in descending order by weight.
- Official generic names only: “elastane,” not “Lycra.” “Polycotton” is not a legal fiber name.
- “100%,” “pure,” or “all” only when the fabric truly is a single fiber.
- Small decorative or elastic parts can be left out with “exclusive of decoration” or “exclusive of elastic.”
Fabric content is the one label fact required in every major market, including the EU and UK, where care and origin are not. The market-by-market rules are in our care label and labeling requirements guide.
What “100 PL” means and the other codes on a spec sheet
Mill paperwork, swatch cards, and many European labels shorten fiber names to two- or three-letter codes.
“100 PL” or “100% PL” means 100% polyester. PES means polyester too.
| Code |
Fiber |
Where you’ll meet it in streetwear |
| CO |
Cotton |
Jersey, French terry, fleece |
| PL / PES |
Polyester |
Fleece blends, sublimation interlock, recycled poly (rPET) |
| EL / EA |
Elastane (spandex, Lycra) |
Rib trims, stretch French terry |
| CV / VI |
Viscose (rayon) |
Tri-blends, drapey tees |
| PA |
Polyamide (nylon) |
Shells, ripstop, mesh |
| WO |
Wool |
Melton for varsity jacket bodies |
Watch this one
PE is not polyester. PE is polyethylene. If a sheet says “100% PE” for a fleece, ask before you accept the quote.
On our floor, 100% polyester shows up in one main place: our polyester interlock, 160-200 gsm, built for edge-to-edge sublimation prints.
Sublimation only works on polyester, so a sublimation tee has to be 100% PL. You can see where it sits in our fabric library.
One rule for your own label: codes belong on spec sheets, not on the sewn-in tag. Your legal label uses the full generic name, “100% polyester,” not “100 PL.”
How to determine fabric content: the Paper–Flame–Lab Check
You can’t see fiber content. A 100% cotton jersey and a 60/40 cotton/poly can look and feel close.
Here’s how to find out what you actually have, from cheapest to most certain.
01 · Paper
Read the paperwork
Check the mill spec sheet, the swatch card, or the fabric test report. The supplier should state the exact split in writing. “Cotton-rich” doesn’t count.
Sending us your own fabric? Send the mill’s spec sheet or test report with the swatch.
Tells you what the supplier claims.
02 · Flame
Run a burn screen
Snip a small piece. Hold it with tweezers over a non-flammable dish, away from anything that can catch.
Cotton burns steadily, smells like paper, and leaves soft grey ash. Polyester shrinks from the flame, melts, gives off black smoke, and leaves a hard bead.
Tells you: natural, synthetic, or a mix. It can’t tell 80/20 from 60/40.
03 · Lab
Order a fiber analysis
Only a lab can confirm the percentages. AATCC TM20 identifies the fibers; AATCC TM20A measures each one’s share by weight. The ISO 1833 series is the international equivalent for blends.
Tells you: the exact split you can defend.
Use the lab when the number has to be right: on a legal label, behind a sustainability claim, or on a customs declaration.
Why it’s worth checking
When you import and sell the garment, the label is usually your legal responsibility, not the factory’s.
Fiber content can also change the tariff line a garment is classified under (see our customs duties guide). And a recycled or organic claim needs proof behind it (see sustainable clothing claims).
The full test panel for shrinkage, color, pilling, and strength is in our fabric testing guide.
Rule of thumb: paper tells you the claim, flame tells you the family, and the lab tells you the number.
Weight (GSM): How much of it?
GSM (grams per square meter) is the industry’s shorthand for heft.
Higher GSM generally means a denser, warmer, more substantial, more “premium-feeling” fabric, and more fabric cost per garment.
It’s the number buyers reach for first because it correlates so strongly with perceived quality.
What we knit and stock, by GSM:
| Fabric |
Our range |
Best for |
| Combed cotton jersey |
180-280 gsm |
Tees |
| Heavyweight jersey |
240-300 gsm |
Boxy tees |
| French terry |
320-400 gsm |
Hoodies, crews |
| Brushed-back fleece |
400-500 gsm |
Premium hoodies, tracksuits |
| Polyester interlock (100% PL) |
160-200 gsm |
Sublimation tees |
Ranges from our fabric library. Every knit we cut is pre-shrunk before cutting.
Two traps live here.
First, GSM without a tolerance is meaningless; bulk will drift, so agree on ±5% (or tighter) and test it.
Second, GSM isn’t the whole quality story. A 300gsm fabric in coarse open-end yarn can feel cheaper than a well-made 240gsm in combed ring-spun.
Weight and yarn together tell the truth.
From our floor
Every incoming fabric roll is checked against the order’s target GSM before a single panel is cut.
Swatches sit in the QC room to condition, then a round cutter punches a 100 cm² disc, and we weigh it. A roll outside the agreed tolerance is flagged before it reaches the cutting table.
One more thing to put on your spec: the finished (post-wash) GSM, not the greige weight. Fabric weight shifts during dyeing and washing.
The way premium feel is built and how to point a customer at it connects to our guide on reading quality cues in a garment.
Construction: How is it knitted?
Construction is the structure the yarn is knitted into.
It’s why two fibers of identical fabric and weight can behave completely differently.
The ones you’ll meet in streetwear:
Single jersey:
The classic tee knit. Light, smooth face, curls at the edges. Different weights cover most tees.
French terry:
Loops on the inside, flat face on the outside. The go-to for crews and lighter hoodies is soft but not fuzzy.
Fleece (brushed-back):
French terry with the loops brushed into a soft nap. Warmer, plusher, heavier is the hoodie standard.
Loopback / loopwheel:
Premium terry knit slowly on wide machines for a denser, more even, more collectible fabric.
Interlock:
Smooth on both faces, more stable and structured than jersey. Good for elevated basics and layers.
Rib (1×1, 2×2);
Stretchy, textured. Used for cuffs, hems, and collars, and as a body fabric for fitted pieces.
The trap: founders treat construction as a game to copy off a competitor.
But construction interacts with weight and finish.
A brushed 350 gsm feels heavier and warmer than an unbrushed 350 gsm terry, even at the same number.
Always read construction and weight together.
Finish: What’s been done to it?
Finishing is everything applied after the fabric is knitted.
It’s the least understood field and one of the most powerful, because it changes the two things customers notice first:
How the fabric feels and how the color behaves.
- Bio/enzyme wash: removes surface fuzz, softens the hand, and reduces pilling. Common on quality cotton.
- Brushing: raises a soft nap (turns terry into fleece). Adds warmth and plushness.
- Peaching/emery: a fine sanding for a peach-skin surface.
- Silicone softener: a slick, soft hand. Pleasant, but it can affect print adhesion. Flag it if you’re printing.
- Anti-pill: a finish (or a better yarn) to resist bobbling on fleece.
- Garment dye: dyeing the finished garment, not the fabric, for a lived-in, tonal look. Beautiful, but expect more shrinkage and shade variance.
- Pre-shrunk: shrinks the knit before cutting, so the fit doesn’t change in the first wash. We run it on every knit we cut.
The trap: finishing quietly moves shrinkage and hand, so a finish change is a spec change.
If a supplier “improves” the softness, ask what they changed and retest shrinkage.
Never assume the sample you loved and the bulk you approved share a finish unless it’s written down.
Rule of thumb:
Composition sets the floor, weight sets the heft, construction sets the behavior, and finish sets the feel.
Change any one, and you’ve changed the fabric even if the headline name stays the same.